Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Water Vapor Transmission = 200 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 50.0 - 200 g/m²/day
3.22 - 12.9 g/100 in²/day
Average value: 126 g/m²/day Grade Count:6
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Water Vapor Transmission 50.0 - 200 g/m²/day
3.22 - 12.9 g/100 in²/day
Average value: 126 g/m²/day Grade Count:6
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Water Vapor Transmission 100 - 200 g/m²/day
6.44 - 12.9 g/100 in²/day
DIN EN 12086
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Water Vapor Transmission 80.0 - 200 g/m²/day
5.15 - 12.9 g/100 in²/day
DIN EN 12086
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..