Material Notes:
Pétromont HDPE 2200 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This resin can be used in a mono layer or co-extrusion resin in applications requiring improved film stiffness and barrier properties, such as in Deli Wrap, cereal box liner, etc.Pétromont HDPE 2200 is an intermediate molecular weight resin offering an excellent combination of maximum barrier properties and stiffness with no detectable taste and odour as well as good extrusion characteristics.
Physical Properties Metric English Comments
Density 0.961 g/cc
0.0347 lb/in³
ASTM D1505
Water Vapor Transmission 4.30 g/m²/day
0.277 g/100 in²/day
24 hrs, 37.8°C, 90% R.H.; ASTM E96
Oxygen Transmission 0.00450 cc-mm/m²-24hr-atm
0.0114 cc-mil/100 in²-24hr-atm
Dry; ASTM D1434
Nitrogen Transmission 0.00160 cc-mm/m²-24hr-atm
0.00406 cc-mil/100 in²-24hr-atm
Dry; ASTM D1434
Carbon Dioxide Transmission 0.0240 cc-mm/m²-24hr-atm
0.0610 cc-mil/100 in²-24hr-atm
Dry; ASTM D1434
Melt Flow 0.70 g/10 min
0.70 g/10 min
I<sub>2</sub>; ASTM D1238
50 g/10 min
50 g/10 min
I<sub>21</sub>; ASTM D238
Thermal Properties Metric English Comments
Melting Point 133 °C
271 °F
Petromont
Crystallization Temperature 119 °C
246 °F
Petromont
Vicat Softening Point 130 °C
266 °F
ASTM D1525