Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.0227 bar @Temperature 20.0 °C |
17.0 torr @Temperature 68.0 °F |
|
LG Chemical IM810 Acrylic impact modifier Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for pro.. |
|||
Vapor Pressure | 0.0227 bar @Temperature 20.0 °C |
17.0 torr @Temperature 68.0 °F |
|
LG Chemical IM812 Acrylic impact modifier Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for pro.. |
|||
Vapor Pressure | 0.0227 bar @Temperature 25.0 °C |
17.0 torr @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® HT110 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service tem.. |