Polymer Property : Vapor Pressure = 0.0227 bar Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.0227 bar

@Temperature 20.0 °C
17.0 torr

@Temperature 68.0 °F
LG Chemical IM810 Acrylic impact modifier
Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for pro..
Vapor Pressure 0.0227 bar

@Temperature 20.0 °C
17.0 torr

@Temperature 68.0 °F
LG Chemical IM812 Acrylic impact modifier
Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for pro..
Vapor Pressure 0.0227 bar

@Temperature 25.0 °C
17.0 torr

@Temperature 77.0 °F
Solvay Specialty Polymers Galden® HT110 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service tem..