Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 127 - 635 microns
5.00 - 25.0 mil
Alcoa KAMA 1120 Prime AntiFog OPS, Sheet  (discontinued **)
CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati..
Thickness 127 - 635 microns
5.00 - 25.0 mil
Alcoa KAMA 1200 Utility Clear OPS, Sheet  (discontinued **)
CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati..
Thickness 127 - 635 microns
5.00 - 25.0 mil
Alcoa KAMA 1500 Freezer Modified OPS  (discontinued **)
CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati..
Thickness 38.1 - 635 microns
1.50 - 25.0 mil
Technetics Group PLASTOLON™ Unsintered PTFE tape  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Thickness 127 - 635 microns
5.00 - 25.0 mil
Alcoa KAMA 1100 Prime Clear OPS, Sheet  (discontinued **)
CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati..