Polymer Property : Thickness = 610 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 508 - 610 microns
20.0 - 24.0 mil
Overall
Arlon 30090R022 0.022" (0.559 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The d..
Thickness 508 - 610 microns
20.0 - 24.0 mil
Side 1
Arlon 30090R022 0.022" (0.559 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The d..