Polymer Property : Thickness = 109 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 109 microns
4.30 mil
Hexcel® HexForce™ 1520 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 109 microns
4.30 mil
Hexcel® HexForce™ 1675 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 109 microns
4.30 mil
Total Thickness
3M 9456 Double Coated Tapes with Adhesive 340
3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t..
Thickness 109 microns
4.30 mil
Tape
3M 9738 Double Coated Splicing Tape
3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres..
Thickness 109 microns
4.30 mil
Tape
3M 9738R Double Coated Splicing Tape
3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres..
Thickness 109 microns
4.30 mil
Total
3M CN-3190 EMI Shielding Tape
3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by..
Thickness 109 microns
4.30 mil
Liner; ASTM D3752
3M 8437 Two-Sided Metalized
3M™ Metalized Polyester Tape 8437 is comprised of relatively thin polyester backing with a metalized coating on both sides of the film providing a mirror-like finish with low emissivity and a versa..
Thickness 109 microns
4.30 mil
Backing
3M CN-4190 EMI Shielding Tape
3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by..
Thickness 109 microns
4.30 mil
Backing
3M X-7001 EMI Shielding Tape
3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by..