3M 8437 Two-Sided Metalized

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 8437 Two-Sided Metalized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Metalized Polyester Tape 8437 is comprised of relatively thin polyester backing with a metalized coating on both sides of the film providing a mirror-like finish with low emissivity and a versatile, long lasting acrylic adhesive. 3M tape 8437 is supplied on a silicone coated release liner for easy handling. The liner also allows for large area applications and die-cutting custom shapes. The liner also provides for additional stiffness and application ease when applying 3M tape 8437 in narrow gaps.Information provided by 3M
Physical Properties Metric English Comments
Thickness 22.9 microns
0.900 mil
Backing; ASTM D3752
53.3 microns
2.10 mil
Total; ASTM D3752
109 microns
4.30 mil
Liner; ASTM D3752
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ASTM D3759
Elongation at Break 70 %
70 %
ASTM D3759
Peel Strength 0.438 kN/m
2.50 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Transparent acrylic
Appearance Silver