Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1020 - 57150 microns | 40.2 - 2250 mil | |
Parker Chomerics WIN-SHIELD™ G (Glass) EMI Shielded Window Description: Parker Chomerics glass windows are designed to offer substrates that provide the hardest surface for resistance to scratching and high temperature applications. Our glass products are .. |
|||
Thickness | 1020 microns | 40.2 mil | Standard |
GrafTech GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material GRAFOIL® GTB flexible graphite sheet is a gasketing material containing no binders or fillers. Standard industrial grade GTB flexible graphite has an oxidation/corrosion inhibitor and is typicall.. |
|||
Thickness | 1020 microns | 40.2 mil | |
Hexcel® HexForce™ 7597 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 1020 microns | 40.0 mil | |
Zircar Refractory Composites SIL-3 Silica Cloth ZIRCAR Type SIL Silica Cloths consists of high temperature non textured amorphous silica fiber yarn, woven into an extremely strong fabrics. These non preshrunk textiles are ideal for applications .. |
|||
Thickness | 1020 microns | 40.0 mil | |
Daikin NEOFLON AF-1000 PFA Film NEOFLON PFA film is a high performance film made from tetrafluoroethylene and perfluoroalkyl vinyl ether (PFA).Information provided by Daikin Industries. |
|||
Thickness | 1020 microns | 40.0 mil | Rubber |
Arlon 30400R040 0.04" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
Thickness | 1020 microns | 40.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 32570R040 0.040" (1.02 mm) Uncured Silicone Rubber with Fiberglass Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
Thickness | 1020 microns | 40.0 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51586R052 0.052" (1.32 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothInterleave: Polyethylene.. |
|||
Thickness | 1020 microns | 40.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55142R040 0.040" (1.02 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be use.. |
|||
Thickness | 1020 microns | 40.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55146R040 0.040"(1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sil.. |
|||
Thickness | 1020 microns | 40.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 61089R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Denier Vectran HS Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 1000 Denier HS Appearance: Red silicone gum on fabricThis data represents t.. |
|||
Thickness | 1020 microns | 40.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 940-15R##-P0 0.040" (1.02 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1.5” Wide Rectangular 1.5 inch wide, 40 mil thick, Red, Rectangular cross-section, Self-f.. |
|||
Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon HSLW401R##-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: High Strength, 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicate.. |
|||
Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-012 |
Arlon LW40125B12-P0 0.040" Self-Fusing Silicone Rubber Tape 1.25 inches wide, 40 mil thick, black, triangular cross-section, self-fusing silicone tape. Product is supplied in 12 yard long roll lengths.Design/Construction:Rubber: Cured Self-fusing Silicone R.. |
|||
Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW401B##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW401B##-P2 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW401C##FR-P1 0.040" (1.02 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Brown, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW401R##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i.. |
|||
Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW401R##-P2 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i.. |
|||
Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW401Y##-M1 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Yellow, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll lengt.. |
|||
Thickness | 1020 microns | 40.0 mil | Dry |
3M Scotchkote™ UV 840 Urethane Coating Scotchkote Urethane Coating UV 840 has been developed to provide a durable gloss finish for use as the final coat of 3M coating systems in the construction and transport industries, where an ease of.. |
|||
Thickness | 1020 microns | 40.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 32400R040 0.040" (1.02 mm) Uncured Silicone Rubber on PET Carrier Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material.. |
|||
Thickness | 1020 microns | 40.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 32400R040 0.040" (1.02 mm) Uncured Silicone Rubber on PET Carrier Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material.. |
|||
Thickness | 1020 microns | 40.0 mil | Total |
3M 4411B Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Thickness | 1020 microns | 40.0 mil | Total |
3M 4411G Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Thickness | 1020 microns | 40.0 mil | Total |
3M 4411N Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Thickness | 1020 microns | 40.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55586R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEAppearance: Red silicone gum and rubber on fiberglass clothThis data .. |
|||
Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW401B##-P0 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-012 |
Arlon RBLW401R##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths. ## in the product number indicates roll length in yards.. |
|||
Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-012 |
Arlon RBLW401X##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths. ## in the product number indicates roll length in yards.. |