Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 10.0 - 15.0 microns | 0.394 - 0.591 mil | Fired |
Lord Adhesives Metech 7806A Cermet Resistor Overglaze Composition Resistor overglaze composition 7806A is an acid resistant, laser trimable glaze designed to be printed and fired over thick film resistors. 7806A improves the stability of laser or air-abrasive trim.. |
|||
Thickness | 13.0 - 15.0 microns | 0.512 - 0.591 mil | Gauge |
UBE 1024FDX41 Nylon 6 BOPA Film Specialties: Excellent processing stabilityProcessing: Best for BOPAApplications: BOPA film (T-die)Information provided by UBE. |