Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FF D0 Very Low Density Polyethylene Clearflex FF D0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FF D0 are highly transparent, have excellent sealing properties,.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FG 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FG 106 are characterized by .. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 336 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, slip agent, antiblocking agent and processing aid, suitable for blown film extrusion.Films obtain.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FG 368 Octene Comonomer Linear Low Density Polyethylene Clearflex FG 368 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 368 ar.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® H&T FHH 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex H&T FHH 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidant, suitable for blown film extrusion.Films obtained from Clearflex H&T FHH 508 show good op.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 208 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LFH.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® H&T LFH 238 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 238 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion. It contains slip and antiblocking a.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Eraclene® FA 706 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 706 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Films manufactured with Eraclene FA 706 show good processability t.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Eraclene® FB 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FB 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Eraclene® FC 82 High Density Polyethylene - Blown Film Extrusion Eraclene FC 82 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully co.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® CM 50 Butene Copolymer Linear Low Density Polyethylene Flexirene CM 50 is a butene copolymer with medium density (C4-LLDPE), with antioxidants, suitable for cast film extrusion.Main Applications: Flexirene CM 50 is a highly stiff product and it is reco.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FF 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex FF 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FF 106 are characterized by .. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FG B0 Very Low Density Polyethylene Clearflex FG B0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FG B0 are highly transparent, have good sealing properties, even.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Average value: 32.1 microns Grade Count:41 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum.. |
|||
Thickness | 10.0 - 75.0 microns | 0.394 - 2.95 mil | Average value: 25.4 microns Grade Count:88 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Thickness | 10.0 microns | 0.394 mil | |
LG Chemical LUTENE-H FE0070 HDPE LUTENE-H FE0070 is mainly intended for the extrusion of blown film with high mechanical properties for the manufacture of "T-Shirt" grocery sacks, can liners. Especially, LUTENE-H FE0070 resin can b.. |
|||
Thickness | 10.0 - 13.0 microns | 0.394 - 0.512 mil | Fired |
Lord Adhesives Metech 3615 Platinum Gold Conductor Composition Platinum gold conductor composition 3615 is a mixed bond conductor designed for military, aerospace, and other high reliability applications that require soldered connections. This composition is de.. |
|||
Thickness | 10.0 microns | 0.394 mil | Fired |
Lord Adhesives Metech 7801 Cermet Resistor Overglaze Composition Resistor overglaze composition 7801 is a laser trimable, green colored glaze designed to be printed and fired over thick film resistors. 7801 improves the stability of laser or air-abrasive trimmed .. |
|||
Thickness | 10.0 - 15.0 microns | 0.394 - 0.591 mil | Fired |
Lord Adhesives Metech 7806A Cermet Resistor Overglaze Composition Resistor overglaze composition 7806A is an acid resistant, laser trimable glaze designed to be printed and fired over thick film resistors. 7806A improves the stability of laser or air-abrasive trim.. |
|||
Thickness | 10.0 - 30.0 microns | 0.394 - 1.18 mil | |
Möller Medical TafSkin 103 NanoCoating Highly flexible, non-abrasive, chemical-resistant PTFE coating with very good easy-to-clean properties, biocompatible.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 10.0 - 30.0 microns | 0.394 - 1.18 mil | cured |
Gwent Electronic Materials C2121119D9 Nanocopper based Paste This product is a nanocopper based paste that is designed for flat bed screens. The product is compatible with printing on PET substrates such as the DuPont Melinex ST-505. Produced using nano-par.. |
|||
Thickness | >= 10.0 microns | >= 0.394 mil | DIN 53353 |
Stanelco Bioplast® GS 2189 Biodegradable Plastic Bioplast 2189 is a product that is optimised for sheet extrusion, injection and compression moulding. It is always biodegradable and readily compostable in thin sections, this material is useable i.. |
|||
Thickness | 10.0 - 120 microns | 0.394 - 4.72 mil | |
BASF Ecovio® C2332 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2332 is our biodegradable film product containing 18% renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic.. |
|||
Thickness | 10.0 microns | 0.394 mil | |
Applied Nanostructured Solutions Carbon NanoStructure Encapsulated Flakes Carbon NanoStructure (CNS) Encapsulated Flakes are a unique form of carbon nanotubes, produced using a proprietary ANS process. The ANS process creates cross-linked multiwall carbon nanotube-based n.. |
|||
Thickness | >= 10.0 microns | >= 0.394 mil | |
Total XSene® HD55110 High Density Polyethylene - Blown Film HDPE HD55110 is a bimodal high density polyethylene with a particular molecular design developed with Total Petrochemicals Double Loop Technology™.HDPE HD55110 has been especially designed for appl.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |
|||
Thickness | 10.0 microns | 0.394 mil | Cured, Printed through 230 stainless steel mesh with 13 micron emulsion |
Gwent Electronic Materials C2000802P2 Carbon Graphite Ink This product is designed to be used for screen-printing working electrodes. This ink has been optimized to give superior electrochemical performance. It combines good line definition and good electr.. |