Melt Flow 800 g/10 min

@Load 2.16 kg,
Temperature 190 °C
800 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
DuPont Elvax® 205W Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® 205W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p..
Melt Flow 800 g/10 min
800 g/10 min
Exxon Method
ExxonMobil Escorene® LD-770 Very High Flow EVA Resin for Specialty Applications  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A relatively low viscosity ethylene vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance, at the same viscosity of..
Melt Flow 800 g/10 min
800 g/10 min
GB/T 3682-2000
Sichuan Deyang Haton® hb DL Polyphenylene Sulfide Resin
Extrusion, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD
Melt Flow 800 g/10 min
800 g/10 min
GB/T 3682-2000
Sichuan Deyang Haton® hb Polyphenylene Sulfide Resin
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD
Melt Flow 800 g/10 min

@Load 2.16 kg,
Temperature 230 °C
800 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Borealis Borflow™ HL508FB Polypropylene Homopolymer
Borflow HL508FB is a polypropylene homopolymer grade intended for fiber applications characterized by narrow molecular weight distribution, controlled rheology, easy processability, optimal product ..
Melt Flow 800 g/10 min

@Load 2.16 kg,
Temperature 230 °C
800 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Total PPS 15080 S01 Polypropylene, Homopolymer Fiber Grade
Polypropylene PPS 15080 S01 is a high melt flow rate homopolymer with a very narrow molecular weight distribution.Polypropylene PPS 15080 S01 is intended for the extrusion of fine fibers with the me..
Melt Flow 800 g/10 min

@Load 2.16 kg,
Temperature 190 °C
800 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Escorene® UL 8705 Adhesive Application Resin
Escorene Ultra UL 8705 is a relatively low viscosity, 27.6% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has ..
Melt Flow 800 g/10 min

@Load 2.16 kg,
Temperature 190 °C
800 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Escorene® UL 8705E Adhesive Application Resin
Escorene Ultra UL 8705 is a relatively low viscosity, 29% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has go..