Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 800 g/10 min @Load 2.16 kg, Temperature 190 °C |
800 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 205W Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 205W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p.. |
|||
Melt Flow | 800 g/10 min | 800 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-770 Very High Flow EVA Resin for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A relatively low viscosity ethylene vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance, at the same viscosity of.. |
|||
Melt Flow | 800 g/10 min | 800 g/10 min | GB/T 3682-2000 |
Sichuan Deyang Haton® hb DL Polyphenylene Sulfide Resin Extrusion, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Melt Flow | 800 g/10 min | 800 g/10 min | GB/T 3682-2000 |
Sichuan Deyang Haton® hb Polyphenylene Sulfide Resin Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Melt Flow | 800 g/10 min @Load 2.16 kg, Temperature 230 °C |
800 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Borflow™ HL508FB Polypropylene Homopolymer Borflow HL508FB is a polypropylene homopolymer grade intended for fiber applications characterized by narrow molecular weight distribution, controlled rheology, easy processability, optimal product .. |
|||
Melt Flow | 800 g/10 min @Load 2.16 kg, Temperature 230 °C |
800 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPS 15080 S01 Polypropylene, Homopolymer Fiber Grade Polypropylene PPS 15080 S01 is a high melt flow rate homopolymer with a very narrow molecular weight distribution.Polypropylene PPS 15080 S01 is intended for the extrusion of fine fibers with the me.. |
|||
Melt Flow | 800 g/10 min @Load 2.16 kg, Temperature 190 °C |
800 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® UL 8705 Adhesive Application Resin Escorene Ultra UL 8705 is a relatively low viscosity, 27.6% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has .. |
|||
Melt Flow | 800 g/10 min @Load 2.16 kg, Temperature 190 °C |
800 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® UL 8705E Adhesive Application Resin Escorene Ultra UL 8705 is a relatively low viscosity, 29% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has go.. |