Material Notes:
Medium viscosity BgVV and FDA - injection molding grade, impact modified, specially for chocolate molds, light colors only.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Water Absorption 0.35 %
0.35 %
Saturation in water
Moisture Absorption at Equilibrium 0.15 %
0.15 %
Equilibrium at 50% RH
Water Absorption at Saturation 0.35 %
0.35 %
Melt Flow 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 6.0 %
6.0 %
Tensile Modulus 2.20 GPa
319 ksi
Charpy Impact Unnotched NB
NB
Thermal Properties Metric English Comments
Vicat Softening Point 145 °C
293 °F