Physical Properties Metric English Comments
Melt Flow 48.3 g/10 min

@Load 5.00 kg,
Temperature 300 °C
48.3 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics NORYL HFM3015P PPE+PS (Asia Pacific)
30% GF/MF filled FR PPE/PS blend
Melt Flow 48.3 g/10 min

@Load 5.00 kg,
Temperature 235 °C
48.3 g/10 min

@Load 11.0 lb,
Temperature 455 °F
ASTM D1238
Cresset Powers Cress-Alon™ NE2740 4% Nano Clay Loaded, 2.7 r.v. Compounding Grade Nylon 6, 50% RH
Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib..
Melt Flow 48.3 g/10 min

@Load 5.00 kg,
Temperature 235 °C
48.3 g/10 min

@Load 11.0 lb,
Temperature 455 °F
ASTM D1238
Cresset Powers Cress-Alon™ NE2740 4% Nano Clay Loaded, 2.7 r.v. Compounding Grade Nylon 6, Dry As Molded
Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib..