Physical Properties Metric English Comments
Melt Flow 26 - 36 g/10 min

@Load 5.00 kg,
Temperature 365 °C
26 - 36 g/10 min

@Load 11.0 lb,
Temperature 689 °F
ASTM D1238
Solvay Specialty Polymers Radel® R-5900 Polyphenylsulfone (PPSU)
Radel® R-5900 polyphenylsulfone (PPSU) offers medium melt viscosities for long flow lengths and greater injection molding ease. It also provides exceptional hydrolytic stability and toughness tha..
Melt Flow 30 - 36 g/10 min

@Temperature 230 °C
30 - 36 g/10 min

@Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene
DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman.
Melt Flow 30 - 36 g/10 min

@Temperature 230 °C
30 - 36 g/10 min

@Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene
DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman.
Melt Flow 30 - 36 g/10 min

@Temperature 230 °C
30 - 36 g/10 min

@Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene
DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman.
Melt Flow 30 - 36 g/10 min

@Temperature 230 °C
30 - 36 g/10 min

@Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene
DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman.
Melt Flow 30 - 36 g/10 min

@Temperature 230 °C
30 - 36 g/10 min

@Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene
DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman.
Melt Flow 30 - 36 g/10 min

@Temperature 230 °C
30 - 36 g/10 min

@Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene
DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman.
Melt Flow 24 - 36 g/10 min
24 - 36 g/10 min
Asahi Glass Fluon® P-62XP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Melt Flow 24 - 36 g/10 min
24 - 36 g/10 min
Asahi Glass Fluon® P-830UP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..