Material Notes:
Description: Antistatic PolycarbonateInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
ASTM D955
Melt Flow 120 g/10 min

@Load 3.80 kg,
Temperature 230 °C
120 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 56.2 MPa
8150 psi
chs 2 in/min; ASTM D638
Flexural Strength 76.297 MPa
11066 psi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
0.125 in bar; ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+12 ohm
1.00e+12 ohm
per cm square at 50% humidity; ASTM D257