Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.75 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.75 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylac® EX28 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 1.75 g/10 min | 1.75 g/10 min | ASTM D1238 |
I. Stern WC-102 General Purpose Crystal Polystyrene Features:Good Processing CharacteristicsUL Classification 94 HBExcellent Water ClarityComplies with FDA Title 21 CFR 177.1640ApplicationsExtrusion FoamDisplaysInformation provided by I. Stern & Co. .. |
|||
Melt Flow | 1.75 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.75 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Micropol Isoplas P381 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Melt Flow | 1.75 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.75 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Fusabond® E226 Polymer Modifier DuPont™ Fusabond® E226 is a anhydride modified polyethylene. Uses: Wire & Cable Applications Polymer Modifier Fusabond E226 resin conforms with the Code of Federal Regulations, Title 21, Paragra.. |