Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 95 SUS | 95 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® AA Cooker & Valve Oil, High Temperature Water Resistant Food Grade ISO 220 Description: ANDEROL PQ AA Cooker & Valve Oil is a white mineral oil based product that meets the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Cooker &.. |
|||
Saybolt Viscosity at 210°F | 95 SUS | 95 SUS | |
ConocoPhillips Hydroclear® 220 Wet Gas Compressor Fluid ISO 220 Description: Conoco Hydroclear® Wet Gas Compressor Fluid is designed to lubricate rotary screw and reciprocating compressors in natural gas service. Conoco's high-quality, hydrocracked base oil.. |
|||
Saybolt Viscosity at 210°F | 95 SUS | 95 SUS | |
ChevronTexaco ISO 220 Cylinder Oil W FeaturesChevron Cylinder Oils W are designed to meet the needs of emulsifying cylinder oils.Chevron Cylinder Oils W provide excellent metal wettability. The combination of oil emulsibility and metal.. |
|||
Saybolt Viscosity at 210°F | 95 SUS | 95 SUS | |
ConocoPhillips 220M Gear Oil AGMA Lubricant No. 5EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |