Category Fluid , Lubricant , White Mineral Oil (WMO)
Manufacturer ConocoPhillips
Trade Name ANDEROL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips ANDEROL® AA Cooker & Valve Oil, High Temperature Water Resistant Food Grade ISO 220.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ANDEROL PQ AA Cooker & Valve Oil is a white mineral oil based product that meets the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Cooker & Valve Oil provides excellent lubrication to the components of the cooker including ways, bearings and chains. It also will remain on the shuttle gate of high-pressure steam valves. PQ AA Cooker & Valve Oil contains special additives that allow it to perform under the high stress of temperature and moisture. PQ food grade lubricants are approved, recommended and field tested by many OEMs in the food processing, baking, bottling, canning, meat processing and pharmaceutical industries. PQ food grade lubricants are listed by NSF International under “USDA Regulations, Proprietary Substances and Nonfood Compounds.”Information provided by ConocoPhillips.Anderol® is a registered trademark of The Anderol Company.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
60°F; ASTM D-1298
Saybolt Viscosity at 100°F 973 SUS
973 SUS
ASTM D-2161
Saybolt Viscosity at 210°F 95 SUS
95 SUS
ASTM D-2161
Kinematic Viscosity at 40°C (104°F) 210 cSt
210 cSt
ASTM D-445
Kinematic Viscosity at 100°C (212°F) 19.2 cSt
19.2 cSt
ASTM D-445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 72.6 kg
160 lb (mass)
ASTM D-2783
Four Ball Wear 0.450 mm
0.0177 in
1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172
Thermal Properties Metric English Comments
Pour Point -10.0 °C
14.0 °F
ASTM D-97
Flash Point 190 °C
374 °F
ASTM D-92
Descriptive Properties Value Comments
Rust Test Pass