Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 51 SUS
51 SUS
ConocoPhillips Syncon® 46 Synthetic AW Hydraulic Fluid 46
Description: Conoco Syncon Synthetic AW Hydraulic Fluid is a synthetic polyalphaolefin (PAO) antiwear fluid for hydraulic systems that operate at extreme temperatures. It is available in four ISO vi..
Saybolt Viscosity at 210°F 51 SUS
51 SUS
ConocoPhillips Syncon® 46 Synthetic R&O Oil
Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv..
Saybolt Viscosity at 210°F 51 SUS
51 SUS
ChevronTexaco Heavy Duty Synthetic Automatic Transmission Fluid
Texaco Synthetic Automatic Transmission Fluid Heavy Duty delivers value through:Extended drains of up to four times that of a conventional automatic transmission fluid.Protection against the formati..
Saybolt Viscosity at 210°F 51 SUS
51 SUS
See Note 3.
ChevronTexaco Multifak® AFB NLGI Grade 2
Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest tempe..
Saybolt Viscosity at 210°F 51 SUS
51 SUS
ChevronTexaco Synthetic Automatic Transmission Fluid, Heavy Duty
FeaturesChevron Synthetic Automatic Transmission Fluid Heavy Duty is engineered to meet the performance requirements of Allison TES 295 for severe duty and extended drain intervals. It is manufactu..
Saybolt Viscosity at 210°F 51 SUS
51 SUS
ConocoPhillips Hydroclear® MV32 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
Saybolt Viscosity at 210°F 51 SUS
51 SUS
ChevronTexaco Biostar® Hydraulic 32
Texaco Biostar Hydraulic oils deliver value through:Environmental sensitivity — Readily biodegradable formulation supports use in environmentally sensitive applications.Reduced maintenance — Ashle..
Saybolt Viscosity at 210°F 51 SUS
51 SUS
ASTM D445
ChevronTexaco Cetus® PAO 46
Texaco Cetus PAO oils deliver value through:Long lubricant life in high temperature operations — Outstanding thermal and oxidation stability.Extended machinery life and increased compressor efficie..
Saybolt Viscosity at 210°F 51 SUS
51 SUS
ChevronTexaco Sultex® F
Texaco Sultex delivers value through:Heavy duty performance — Texaco Sultex oils are designed for tough machining operations on difficult to machine metals and alloys.Low tool wear — Special compo..