Material Notes:
Texaco Sultex delivers value through:Heavy duty performance — Texaco Sultex oils are designed for tough machining operations on difficult to machine metals and alloys.Low tool wear — Special compounding provides excellent lubricity and antiweld properties.Good surface finishes — Chip welding is highly reduced. Surface of finished parts come out extremely fine, producing high quality work.Texaco Sultex oils are dark, active sulfur, heavy duty cutting oils. They contain highly effective EP and lubricity additives that provide maximum cutting performance. They should not be used to machine copper or its alloys.Texaco Sultex cutting oils:provide excellent cooling and lubrication in a wide range of machining operationsprevent welding of chip and toolprotect the finished work surfaces, tools and machine against rust and corrosionprovide long tool life and excellent surface finishflush chips away from the work areareduce oil mist in high-speed machine toolsTexaco Sultex cutting oils are formulated with paraffinic base stocks with a naturally high viscosity index. These cutting oils have high flash points, minimizing the potential for fireTexaco Sultex oils possess the highest level of EP and antiweld properties.Texaco Sultex D and F are recommended for difficult machining operations, such as tapping, threading, broaching, gear cutting and form grinding. They are suited for machining of ferrous alloys with machinability ratings below 70%Texaco Sultex F contains a higher level of fatty oil to provide good surface finishes in severe machining operations. Texaco Sultex F may also be used to fortify lighter-duty cutting oils for more severe operations.Texaco Sultex oils are also suitable for drawing and stamping operations on difficult to machine metals and alloys.Texaco Sultex oils contain active sulfur that is staining to yellow metals. Texaco Sultex oils should not be used to machine copper and its alloys.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.CPS Number: 221585; MSDS Number: 8904
Physical Properties Metric English Comments
API Gravity 27.1 °
27.1 °
Saybolt Viscosity at 100°F 240 SUS
240 SUS
Saybolt Viscosity at 210°F 51 SUS
51 SUS
Kinematic Viscosity at 40°C (104°F) 46.7 cSt
46.7 cSt
Kinematic Viscosity at 100°C (212°F) 7.3 cSt
7.3 cSt
ASTM Color 8.0
8.0
D
Descriptive Properties Value Comments
Chlorine None
Fatty Oil Present
Phosphorus Present
Sulfur Present