Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 494 SUS | 494 SUS | |
ChevronTexaco FM ISO 100 Lubricating Oil Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr.. |
|||
Saybolt Viscosity at 100°F | 494 SUS | 494 SUS | |
ChevronTexaco Regal® AW 100 Texaco Regal AW oil delivers value through:High Temperature stability provides long lubricant life and resistance to formation of sludge and varnish on bearings and gears.Excellent wear protection p.. |
|||
Saybolt Viscosity at 100°F | 494 SUS | 494 SUS | |
ChevronTexaco Clarity® ISO 100 Paper Machine Oil FeaturesChevron Clarity Paper Machine Oils are the next generation circulating oils for the pulp and paper industry.Chevron Clarity Paper Machine Oils ISO 100, 150, and 220 are formulated with ISOS.. |
|||
Saybolt Viscosity at 100°F | 494 SUS | 494 SUS | |
ChevronTexaco Clarity® ISO 100 Saw Guide Oil FeaturesChevron Clarity Saw Guide Oils are designed to promote longer saw guide and saw blade life in thin kerf saw equipment, when operating in severe service and reduced cooling water modes.Chevro.. |
|||
Saybolt Viscosity at 100°F | 494 SUS | 494 SUS | |
ChevronTexaco Cygnus® 100 Hydraulic Oil Texaco Cygnus Hydraulic Oils deliver value through:High quality control — Enables customer to use lubricants almost as pure as the food being processedHigh performance — Provides lubrication bette.. |
|||
Saybolt Viscosity at 100°F | 494 SUS | 494 SUS | |
ChevronTexaco Starguide™ ISO 100 Texaco Starguide oils deliver value through:Cleaner cutting — Reduce excessive drag that slows cutting.Exceptional performance for low water and low oil consumption saw systems.Excellent low temper.. |