ChevronTexaco FM ISO 100 Lubricating Oil

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name FM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco FM ISO 100 Lubricating Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubricating Oils FM provide performance well above that found in typical white mineral oils often used in the food industry. They contain a special biocide to prevent growth of molds when the product comes in contact with food or water.ApplicationsCirculating oil systemsairline lubricatorsbearing lubrication
Physical Properties Metric English Comments
API Gravity 31.5 °
31.5 °
Viscosity Measurement 105
105
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 494 SUS
494 SUS
Saybolt Viscosity at 210°F 65 SUS
65 SUS
Kinematic Viscosity at 40°C (104°F) 95 cSt
95 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 11.3 cSt
11.3 cSt
ASTM D445
Oxidative Stability >= 15000 hour
>= 15000 hour
Hours to 2.0 mg KOH/g acid number; ASTM D943
Mechanical Properties Metric English Comments
Four Ball Wear 0.440 mm
0.0173 in
Thermal Properties Metric English Comments
Pour Point -9.00 °C
15.8 °F
ASTM D97
Flash Point 260 °C
500 °F
ASTM D92
Descriptive Properties Value Comments
Rust preventative Test Procedure B Pass
Synthetic Sea Water
Vickers V104C Pump Test Total Wear, mg 19.2