Physical Properties Metric English Comments
Apparent Bulk Density 1.65 g/cc
0.0596 lb/in³
Poco Graphite CZR Semiconductor Grade Graphite
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their ..
Apparent Bulk Density 1.65 g/cc
0.0596 lb/in³
Carlisle 201LL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Apparent Bulk Density 1.65 g/cc
0.0596 lb/in³
Carlisle 201HL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..