Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 1.65 g/cc | 0.0596 lb/in³ | |
Poco Graphite CZR Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Apparent Bulk Density | 1.65 g/cc | 0.0596 lb/in³ | |
Carlisle 201LL Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |
|||
Apparent Bulk Density | 1.65 g/cc | 0.0596 lb/in³ | |
Carlisle 201HL Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |