Sharadaa Ceramics REFCAST 80 High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics REFCAST A High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics REFCAST A SUPER High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics REFCAST C SUPER High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Grain Size >= 5000 µm
>= 5000 µm
Sharadaa Ceramics REFCAST Dense Castables
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics REFCAST HA High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics REFCAST K High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics REFCAST LT Dense Castables
Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics REFCAST NORMAL Dense Castables
Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics REFCAST SPECIAL Dense Castables
Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range..
Grain Size >= 5000 µm
>= 5000 µm
Sharadaa Ceramics REFCAST SPL Dense Castables
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Grain Size >= 5000 µm
>= 5000 µm
Sharadaa Ceramics REFCAST SUPER Dense Castables
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics REFCAST SUPER Dense Castables
Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics THERMO PATCH Dense Castables
Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics THERMO PATCH EXCEL High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics ZAP 001 Smart Cast Application
Special Properties: Thermal Shock Slag ResistanceIndustry: FoundryApplication Areas: Foundry LaddleInformation provided by Sharadaa Ceramics Pvt. Ltd.
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics ZAP 005 Smart Cast Application
Special Properties: Non-wetting, Slag and Hot Abrasion ResistanceIndustry: SteelApplication: Trough LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics ZAP 008 Smart Cast Application
Special Properties: Thermal Shock Slag ResistanceIndustry: SteelApplication: Pig Iron Laddle Safety Layer, Sponge Iron Rotary Kiln BackupInformation provided by Sharadaa Ceramics Pvt. Ltd.
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics REFCAST C High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics REFCAST HA PLUS High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Grain Size <= 5000 µm
<= 5000 µm
Sharadaa Ceramics ZAP 013 Smart Cast Application
Special Properties: Low Density, High Strength, Low Thermal ConductivityIndustry: Multi PurposeApplication: All type furnaces as a back up layer, Insulating Burner BlocksInformation provided by Shar..