Sharadaa Ceramics THERMO PATCH Dense Castables

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Sharadaa Ceramics
Trade Name THERMO
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics THERMO PATCH Dense Castables.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range is known for its high strength, low thermal conductivity and requires less maintenance.Information provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density >= 2.50 g/cc
>= 0.0903 lb/in³
Sample, cast, cured, dried at 110°C
Grain Size <= 5000 µm
<= 5000 µm
Mechanical Properties Metric English Comments
Compressive Strength 39.2 MPa

@Temperature 110 °C
5690 psi

@Temperature 230 °F
Cold Crushing
58.8 MPa

@Temperature 110 °C
8530 psi

@Temperature 230 °F
Cold Crushing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1400 °C
2550 °F
Component Elements Properties Metric English Comments
Al2O3 >= 60 %
>= 60 %
Fe2O3 <= 2.0 %
<= 2.0 %
Processing Properties Metric English Comments
Moisture Content 10 - 12 %
10 - 12 %
Descriptive Properties Value Comments
Permanent Linear Change -1.0 - 1.0%