Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 75 - 95 cP | 75 - 95 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE METHYL FOR METALS (75-95 Viscosity) Rapid Bonding Adhesive Palm Lab's Methyl Cyanoacrylate is a one component rapid bonding adhesive ideal for metal surfaces. TURBO FUSE METHYL’s advanced formula is designed to polymerize instantly by absorbing surface moi.. |
|||
Viscosity | 75 cP @Temperature 25.0 °C |
75 cP @Temperature 77.0 °F |
|
Northstar Polymers BNA-005 Polyester Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 75 - 85 cP | 75 - 85 cP | |
Huntsman Araldite ECN 1280 Epoxy Cresol Novolac Weight per Epoxide (EEW, g/eq) 212 to 233. Max color is |
|||
Viscosity | 75 cP @Temperature 25.0 °C |
75 cP @Temperature 77.0 °F |
Solution Viscosity in 5 wt.% Toluene; UBE Method |
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber (Raw Polymer) Description: UBEPOL BR is UBE's line of polybutadiene rubber products. Stabilizer Type: Non-stainingMicrostructure: cis: 98trans: 1vinyl: 1Information provided by UBE. |
|||
Viscosity | 75 - 100 cP @Temperature 23.0 °C |
75 - 100 cP @Temperature 73.4 °F |
|
Master Bond MB302 Cyanoacrylate Adhesive System For rubber & plastic bonding, fills gap to 0.005Information provided by Master Bond Inc. |
|||
Viscosity | 75 - 95 cP | 75 - 95 cP | |
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver.. |
|||
Viscosity | 75 - 200 cP @Temperature 125 °C |
75 - 200 cP @Temperature 257 °F |
542-111 |
Westlake Epolene® N-14 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-14 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Viscosity | 75 - 200 cP | 75 - 200 cP | 542-111 |
Westlake Epolene® N-14P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-14P is a polyethylene (PE) homopolymer powder that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Viscosity | 75 cP @Temperature 25.0 °C |
75 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Eccobond® 1309 General Purpose Catalyst Emerson & Cuming 1309 Eccobond® General Purpose CatalystFaster curing version of 9. Very fast room temperature curing, low viscosity, general purpose. Short working life. Imparts excellent chemical.. |
|||
Viscosity | 75 cP | 75 cP | dynamic |
Dow Corning SYL-OFF® 1181 EMULSION COATING Syl-Off® 1181 Emulsion Coating is a 40% solids emulsion of a silanol functional silicone polymer and multifunctional crosslinker in water. Highly robust emulsion coating recommended for use with di.. |
|||
Viscosity | 75 cP | 75 cP | dynamic |
Dow Corning SYL-OFF® 7924 CATALYST EMULSION Syl-Off® 7924 Catalyst Emulsion is a 40% solids emulsion of vinyl functional polymer and platinum catalyst in water. An extended bath-life catalyst recommended where long bath-life is required.Info.. |
|||
Viscosity | 75 cP | 75 cP | dynamic |
Dow Corning SYL-OFF® 7950 EMULSION COATING Syl-Off® 7950 Emulsion Coating is a 40% solids emulsion of a vinyl endblocked silicone polymer in water. The coating is pre-formulated with crosslinker. Provides premium release performance and fas.. |
|||
Viscosity | 75 cP | 75 cP | Dynamic |
Dow Corning SYL-OFF® PMCP7924 Catalyst Emulsion Syl-Off® 7924 Catalyst Emulsion is a 40% solids emulsion of vinyl functional polymer and platinum catalyst in water. An extended bath-life catalyst recommended where long bath-life is required.Info.. |
|||
Viscosity | 75 cP | 75 cP | Dynamic |
Dow Corning SYL-OFF® PMCP7950 Emulsion Coating Syl-Off® 7950 Emulsion Coating is a 40% solids emulsion of a vinyl endblocked silicone polymer in water. The coating is pre-formulated with crosslinker. Provides premium release performance and fas.. |
|||
Viscosity | 75 cP @Temperature 25.0 °C |
75 cP @Temperature 77.0 °F |
Value represents initial mixed viscosity of components. |
Cytec Conathane® CC-1155 (Conap) Polyurethane Two-component Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Viscosity | 75 cP @Temperature 25.0 °C |
75 cP @Temperature 77.0 °F |
Value represents initial mixed viscosity of components. |
Cytec Conathane® CC-1195 (Conap) Polyurethane Two-component Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Viscosity | 75 cP | 75 cP | |
BASF Lupranate® 5010 Isocyanate Description: Lupranate® 5010 Isocyanate is a prepolymer based on polymeric MDI.Information provided by BASF |
|||
Viscosity | 75 cP | 75 cP | |
BASF Lupranate® 5130 Isocyanate Description: Lupranate® 5130 Isocyanate has the combined characteristics of a liquid carbodiimidemodified isocyanate and a pure MDI prepolymer. The relatively low functionality and high free-NCO of.. |
|||
Viscosity | 75 cP | 75 cP | Part B |
Resinlab® UR3001 Clear Two Part Urethane Encapsulant Resinlab™ UR 3001 is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR 3001 provides excellent environmental p.. |