Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning SYL-OFF® PMCP7924 Catalyst Emulsion

Category Other Engineering Material , Catalyst/Initiator
Manufacturer Dow Corning
Trade Name SYL-OFF®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYL-OFF® PMCP7924 Catalyst Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Syl-Off® 7924 Catalyst Emulsion is a 40% solids emulsion of vinyl functional polymer and platinum catalyst in water. An extended bath-life catalyst recommended where long bath-life is required.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc

@Temperature 25.0 °C
0.990 g/cc

@Temperature 77.0 °F
pH 4.5
4.5
Viscosity 75 cP
75 cP
Dynamic
Descriptive Properties Value Comments
Active Content (%) 40
Color Milky White
Copyright © lookpolymers.com All Rights Reserved