Polymer Property : Viscosity = 675 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 525 - 675 cP
525 - 675 cP
Huntsman Araldite GY 9513 Bisphenol A Epoxy Liquid Resin
Weight per Epoxide (EEW, g/eq) 196 to 205. Max color is 1.Comments/Applications: GY 6010 modified with DY 025 (Epoxide 8). Lower toxicity than typical low viscosity modified epoxy resins. High so..