Huntsman Araldite GY 9513 Bisphenol A Epoxy Liquid Resin

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite GY 9513 Bisphenol A Epoxy Liquid Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 196 to 205. Max color is 1.Comments/Applications: GY 6010 modified with DY 025 (Epoxide 8). Lower toxicity than typical low viscosity modified epoxy resins. High solids and solvent free coatings and floorings.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 525 - 675 cP
525 - 675 cP