Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 525 - 675 cP | 525 - 675 cP | |
Huntsman Araldite GY 9513 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 196 to 205. Max color is 1.Comments/Applications: GY 6010 modified with DY 025 (Epoxide 8). Lower toxicity than typical low viscosity modified epoxy resins. High so.. |
|||
Viscosity | 525 - 1850 cP | 525 - 1850 cP | Thixotropic |
Loctite® 542 Fine Threads Thread Sealant Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p.. |
|||
Viscosity | 525 - 1950 cP | 525 - 1950 cP | Thixotropic |
Loctite® 641 Controlled Strength Retaining Compound RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. .. |
|||
Viscosity | 525 cP @Temperature 25.0 °C |
525 cP @Temperature 77.0 °F |
|
Esstech X-739-0000 Ethoxylated Bis Phenol A Dimethacrylate, C39H56O12 This form of EBPADMA has 8 units of ethoxylation. Increasing the ethoxylated chain length increases the mobility of the molecule and therefore it reactivity and degree of conversion. Listed on the .. |