Polymer Property : Viscosity = 5800 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 4200 - 5800 cP

@Temperature 25.0 °C
4200 - 5800 cP

@Temperature 77.0 °F
Uncured
Resin Technology Group UV-412 Medium Viscosity, High Clarity, UV Curable Adhesive
UV 412 is a high clarity, fast setting UV adhesive. This solvent free adhesive is designed to bond a wide variety of transparent materials, (similar and dissimilar substrates). The high clarity prov..
Viscosity 3100 - 5800 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
3100 - 5800 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2030519P4 Carbon Graphite Ink
This product is designed to be used for screen printed working electrodes. It gives excellent electrochemical performance with good reversibility when using cyclic voltammetry.This ink can be used i..
Viscosity 17.0 - 5800 cP

@Temperature 30.0 - 30.0 °C
17.0 - 5800 cP

@Temperature 86.0 - 86.0 °F
Average value: 1.53e+6 cP Grade Count:21
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..