Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 4200 - 5800 cP @Temperature 25.0 °C |
4200 - 5800 cP @Temperature 77.0 °F |
Uncured |
Resin Technology Group UV-412 Medium Viscosity, High Clarity, UV Curable Adhesive UV 412 is a high clarity, fast setting UV adhesive. This solvent free adhesive is designed to bond a wide variety of transparent materials, (similar and dissimilar substrates). The high clarity prov.. |
|||
Viscosity | <= 4200 cP @Temperature -40.0 °C |
<= 4200 cP @Temperature -40.0 °F |
Apparent Viscosity by Mini-Rotary Viscometer; ASTM D4684 |
ExxonMobil SpectraSyn™ 5 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |
|||
Viscosity | 4200 cP @Temperature -25.0 °C |
4200 cP @Temperature -13.0 °F |
Cold Crank |
ChevronTexaco Drive Train Fluid HD, SAE 10W FeaturesChevron Drive Train Fluids HD are high performance lubricants designed for use in transmissions, final drives, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or Allison C4 .. |
|||
Viscosity | 4200 - 5000 cP @Temperature 35.0 °C |
4200 - 5000 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G211 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 4200 - 5000 cP @Temperature 35.0 °C |
4200 - 5000 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G222 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 4200 cP @Temperature -25.0 °C |
4200 cP @Temperature -13.0 °F |
Cold Crank |
ChevronTexaco SAE 10W Transmission and Drive Train TO-4 Oil Texaco Transmission and Drive Train TO-4 Oils deliver value through:Longer equipment life — Special additives protect metal surfaces against scuffing and wear even under severe operating conditions.. |