Material Notes:
AA-BOND F162 is a thixotropic electrical insulating epoxy adhesive system with low vapor pressure and outgassing characteristics. AA-BOND F162 was specifically developed for fiber optic, laser, photonic and electronic applications requiring excellent electrical insulation in combination with effective thermal dissipation from heat-producing components. AA-BOND F162 is two-part epoxy compound develops strong, durable, stable, high impact thermally conductive bonds at room temperature, and adheres readily to itself, and to metals, many plastics, silica, steatite, alumina, sapphire and other ceramics, glass, and to many other materials. AA-BOND F162 provides excellent resistance to salt solutions, mild acids and alkalis and many other chemicals including petroleum solvents, lubricating oils and alcohol.Appearance: Red Cure Type: Heat cure or Room TemperatureBenefits:Smooth pasteFiber opticLaserPhotonic and electronic applicationsGood electrical insulation Mix Ratio by weight: 100:10/Resin:Hardener Substrates: Metals, Many plastics, Glass, and other materialsTypical Application: ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components.Information provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 2.29 g/cc
2.29 g/cc
uncured
Solids Content 100 %
100 %
uncured
Viscosity 54000 cP
54000 cP
uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
cured
Thermal Properties Metric English Comments
Thermal Conductivity 0.878 W/m-K
6.09 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.10e+15 ohm-cm
2.10e+15 ohm-cm
Dielectric Constant 5.9

@Frequency 1000 Hz
5.9

@Frequency 1000 Hz
Dielectric Strength 16.1 kV/mm
410 kV/in
Dissipation Factor 0.010

@Frequency 1000 Hz
0.010

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 120 - 240 min

@Temperature 65.0 °C
2.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Thixotropic Index 2