Polymer Property : Viscosity = 500000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 90000 - 500000 cP

@Temperature 400 - 400 °C
90000 - 500000 cP

@Temperature 752 - 752 °F
Average value: 324000 cP Grade Count:13
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Viscosity 250000 - 500000 cP

@Temperature 25.0 °C
250000 - 500000 cP

@Temperature 77.0 °F
Uncured
Permabond ES569 Epoxy Resin
PERMABOND® ES569 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces as well as composite materials. The high bond strength of this adhesive allows it to replace me..
Viscosity 300000 - 500000 cP
300000 - 500000 cP
Dynamic
Dow Corning 9041 Silicone Elastomer Blend
A mixture of high molecular weight silicone elastomers (dimethicone crosspolymer) in cyclopentasiloxane for use in skincare, haircare, color cosmetics, suncare, antiperspirants and deodorants, and w..
Viscosity 188000 - 500000 cP
188000 - 500000 cP
Thixotropic
Loctite® Gasket Eliminator® 510 Flange Sealant
Anaerobic GasketingLoctite® 510 High Temperature Rigid Cure Gasket Eliminator® Flange SealantProduct has a temperature range to 400ºF with excellent solvent and chemical resistance. Makes or dre..