Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1600 - 5500 cP | 1600 - 5500 cP | |
Ritelok TL62 Studlock Anaerobic. High Strength studlock for heavy duty items, vibration & stress load. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant |
|||
Viscosity | 1600 - 2500 cP | 1600 - 2500 cP | |
ND Industries High Temperature SuperGlue 362 Medium viscosity with thermal cycling resistance |
|||
Viscosity | 1600 - 3000 cP | 1600 - 3000 cP | Thixotropic |
ND Industries StudGrade® 131 Permanent CT Threadlocker General DescriptionHigh strength threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical Usesstuds and bolts, and threaded pipe fittings.Meets m.. |
|||
Viscosity | 1600 - 2600 cP @Temperature 25.0 °C |
1600 - 2600 cP @Temperature 77.0 °F |
|
Northstar Polymers MPG-062 MDI Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 1600 - 2300 cP @Temperature 180 - 180 °C |
1600 - 2300 cP @Temperature 356 - 356 °F |
Average value: 2080 cP Grade Count:4 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Viscosity | 1600 - 2000 cP | 1600 - 2000 cP | |
Huntsman Araldite GY 9580 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 188 to 198. Max color is 3.Comments/Applications: GY 6010 modified with DY 025 (Epoxide 8). High solids and solvent free coatings and floorings.Data provided by Ciba.. |
|||
Viscosity | 1600 - 2200 cP | 1600 - 2200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-420 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for fo.. |
|||
Viscosity | 1600 - 2000 cP | 1600 - 2000 cP | 20% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-620 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Viscosity | 1600 - 2200 cP | 1600 - 2200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-626 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Viscosity | 1600 - 2200 cP | 1600 - 2200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-632A TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for fo.. |
|||
Viscosity | 1600 - 2200 cP | 1600 - 2200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-632B TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for fo.. |
|||
Viscosity | 1600 - 2200 cP | 1600 - 2200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-632H TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for fo.. |
|||
Viscosity | 1600 - 2200 cP | 1600 - 2200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-690 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Viscosity | 1600 - 2000 cP | 1600 - 2000 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-731 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Non-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for.. |
|||
Viscosity | 1600 - 2000 cP | 1600 - 2000 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-733 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Non-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for.. |
|||
Viscosity | 1600 - 1800 cP | 1600 - 1800 cP | Part A |
Master Bond EP30P Epoxy Bonds Glass, Polycarbonates and Acrylics Description: Master Bond Polymer Adhesive EP30P is a two component, transparent, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is for.. |
|||
Viscosity | 1600 - 7600 cP | 1600 - 7600 cP | Milled Cement; Zeon Test #327 |
Zeon Chemicals Nipol® 1002 Nitrile Elastomer Nipol 1002 is a copolymer of butadiene and acrylonitrile with medium oil resistance. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.The original medium.. |
|||
Viscosity | 1600 - 4800 cP | 1600 - 4800 cP | Unmilled Cement; Zeon Test #328 |
Zeon Chemicals Nipol® 1052 Nitrile Elastomer Nipol 1052 is a copolymer of butadiene and acrylonitrile with medium oil resistance. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.Excellent general p.. |
|||
Viscosity | 1600 cP | 1600 cP | |
Trelleborg Emerson & Cuming Stycast® XT-5038-9 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Viscosity | 1600 - 1800 cP @Temperature 23.0 °C |
1600 - 1800 cP @Temperature 73.4 °F |
|
Master Bond EP30MED USP Class VI Certified Two Component Epoxy System Master Bond EP30Med is a two component, optically clear, low viscosity epoxy resin system for high performance bonding, sealing, coating, and encapsulating. It features excellent physical and electr.. |
|||
Viscosity | 1600 - 1800 cP | 1600 - 1800 cP | |
Epoxyset Epoxibond EB-130M-1 Unfilled Epoxy Adhesive A two-component, non-hazmat, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc. |
|||
Viscosity | 1600 cP | 1600 cP | Dynamic |
Dow Corning 2-2677 Performance Modifier Surface active silicone designed for reducing surface tension in silicone emulsions and improving drainage in pulp brownstock washing.Information provided by Dow Corning |
|||
Viscosity | 1600 cP @Temperature 180 °C |
1600 cP @Temperature 356 °F |
Modified Bitumen Property in waterproof membranes (150/200 bitumen + 12% polymer) |
Dynasol Calprene® 419 Thermoplastic Rubber SBS Dry Calprene 419 is a 70/30 Butadiene/Styrene thermoplastic copolymer, polymerized in solution and has a radial structure.This product is available in:Calprene 419 porous crumbCalprene 419M powder form .. |
|||
Viscosity | 1600 cP @Temperature 180 °C |
1600 cP @Temperature 356 °F |
Modified Bitumen Property in waterproof membranes (150/200 bitumen + 12% polymer) |
Dynasol Calprene® 501 Thermoplastic Rubber SBS Dry Calprene 501 is a 69/31 Butadiene/Styrene thermoplastic copolymer, polymerized in solution and having a linear structure.This product is available in:C 501 porous crumbC 501C porous pelletC 501M pow.. |
|||
Viscosity | 1600 cP | 1600 cP | |
Abatron AboCast 8110-2/AboCure 8110-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Viscosity | 1600 - 2000 cP | 1600 - 2000 cP | |
Abatron AboCast/AboCure 8109-3 Low viscosity, RT cure. Easy processing.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140.. |
|||
Viscosity | 1600 - 2000 cP | 1600 - 2000 cP | uncured |
Atom Adhesives AA-BOND F131 Epoxy Adhesive AA-BOND F131 is two parts fiber-optic adhesive used for terminating ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components. AA-BOND F131 produces a typical .. |