Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 100000 - 200000 cP | 100000 - 200000 cP | |
Palm Labs Adhesives Turbo Anti-Seize Aluminum Paste TURBO ANTI-SEIZE – ALUMINUM is a gray, viscous metallic paste which may be used on all bolts, studs, value shafts, value assemblies, transmission shafts, and other types of assembly work where prot.. |
|||
Viscosity | 100000 - 200000 cP | 100000 - 200000 cP | |
Palm Labs Adhesives Turbo Anti-Seize Copper Paste TURBO ANTI-SEIZE – COPPER is a copper, viscous metallic paste which may be used on all bolts, studs, value shafts, value assemblies, transmission shafts, and other types of assembly work where prot.. |
|||
Viscosity | 100000 - 200000 cP | 100000 - 200000 cP | |
Palm Labs Adhesives Turbo Anti-Seize Nickel Paste TURBO ANTI-SEIZE – NICKEL is a gray, viscous metallic paste which may be used on all bolts, studs, value shafts, value assemblies, transmission shafts, and other types of assembly work where protec.. |
|||
Viscosity | 70000 - 200000 cP | 70000 - 200000 cP | |
Lord Adhesives 510 Fast Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Viscosity | 140000 - 200000 cP | 140000 - 200000 cP | |
Master Bond Supreme 10HTCL Epoxy for Cryogenic Applications Description: Master Bond Supreme 10HTCL features a blend of performance properties including both high shear and peel strengths along with convenient handling. This one component system is formulate.. |
|||
Viscosity | 65000 - 200000 cP | 65000 - 200000 cP | Thixotropic |
Loctite® Gasket Eliminator® 509 Flange Sealant Anaerobic GasketingLoctite® 509 Flexible Cure Gasket Eliminator® Flange SealantProduct withstands minor flange movements caused by vibrations. It will not run when applied to vertical surfaces. F.. |