Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 65000 cP | 65000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East) Super high flow FR PBT grade with 15% Glass reinforced |
|||
Viscosity | 65000 - 75000 cP @Temperature 23.0 °C |
65000 - 75000 cP @Temperature 73.4 °F |
|
Master Bond Supreme 45HT Toughened Heat Resistant Two Component Epoxy Adhesive Master Bond Polymer Supreme 45HT is a two component epoxy adhesive featuring an attractive balance of superior shear and peel strengths for high performance structural bonding and coating suitable f.. |
|||
Viscosity | 65000 cP @Temperature 25.0 °C |
65000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond F118 Fiber Optic Epoxy Adhesive TRA-BOND F118 is an impact resistant, fiber-optic adhesive designed for use in any optical connector. This two-part epoxy remains at a constant viscosity for a minimum of 30 minutes. This allows mor.. |
|||
Viscosity | 65000 cP @Temperature 25.0 °C |
65000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond F118CLR Fiber Optic Epoxy Adhesive TRA-BOND F118CLR is an impact resistant, fiber-optic adhesive designed for use in any optical connector. This two-part epoxy remains at a constant viscosity for a minimum of 30 minutes. This allows .. |
|||
Viscosity | 65000 cP @Temperature 25.0 °C |
65000 cP @Temperature 77.0 °F |
Mixed (cp #52, 5 rpm) |
Tra-Con Tra-Bond FDA23 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-23 is a high viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admini.. |
|||
Viscosity | 65000 cP @Temperature 25.0 °C |
65000 cP @Temperature 77.0 °F |
Mixed (cp #52, 10 rpm) |
Tra-Con Tra-Duct 2979 Microelectronic Conductive Epoxy Adhesive TRA-DUCT 2979 is a fast curing one-part epoxy adhesive with superior electrical conductivity and bonding capability. It has been shown to retain these properties through hundreds of hours of rapid t.. |
|||
Viscosity | 65000 cP @Temperature 25.0 °C |
65000 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Eccobond® 2780-45 One-Component High Temperature Performance Epoxy Adhesive Emerson & Cuming 2780-45 Eccobond® One-Component High Temperature Performance Epoxy AdhesiveFilled, pourable, high temperature resistant, epoxy adhesive. Long term resistance to boiling glycol. Exc.. |
|||
Viscosity | 65000 cP | 65000 cP | |
Trelleborg Emerson & Cuming Stycast® 2850FT-FR/11 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Viscosity | 65000 - 200000 cP | 65000 - 200000 cP | Thixotropic |
Loctite® Gasket Eliminator® 509 Flange Sealant Anaerobic GasketingLoctite® 509 Flexible Cure Gasket Eliminator® Flange SealantProduct withstands minor flange movements caused by vibrations. It will not run when applied to vertical surfaces. F.. |
|||
Viscosity | 65000 - 90000 cP @Temperature 23.0 °C |
65000 - 90000 cP @Temperature 73.4 °F |
1 rpm |
Epoxy Technology EPO-TEK® E2116 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E2116 is a two component, silver-filled and stencil printable electrically conductive adhesive for bonding SMDs onto PCB and substrates. Can be used as a “lead-free”.. |
|||
Viscosity | 65000 cP | 65000 cP | uncured |
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive AA-DUCT 2979 is a fast curing one part epoxy adhesive with superior electrical conductivity and bonding capability. AA-DUCT 2979 has been shown to retain their properties through hundreds of hours o.. |
|||
Viscosity | 65000 cP | 65000 cP | Mixed; TM R050-12 |
Resinlab® EP1238 Acrylic / Epoxy Hybrid Adhesive Resinlab™ EP1238 is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wetting to.. |
|||
Viscosity | 65000 cP | 65000 cP | Mixed - medium; Resin - 65,000 cP; Hardener - 7,000 cP |
Loctite® Durabond® E-20HP Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Viscosity | 65000 cP | 65000 cP | Mixed; TM R050-12 |
Resinlab® EP1238 Black Acrylic / Epoxy Hybrid Adhesive Resinlab™ EP1238 Black is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wett.. |