Polymer Property : Viscosity = 19000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 7000 - 19000 cP
7000 - 19000 cP
Huntsman MY 720 Multifunctional Resin
Weight per Epoxide (EEW, g/eq) 117 to 134. Color: BrownComments/Applications: Tetra-functional liquid epoxy based on methylene dianiline. Excellent high temperature, chemical and radiation resista..
Viscosity 11000 - 19000 cP

@Shear Rate 100 1/s,
Temperature 25.0 °C
11000 - 19000 cP

@Shear Rate 100 1/s,
Temperature 77.0 °F
Haake VT550 cone and plate viscometer (PK1.1°)
Gwent Electronic Materials C2000107P3 Silver Ink
Silver Ink C2000107P3 is designed as a termination for single layer PZT ceramics. After firing the film has good adhesion and solderability.The ink is in a ready to use form at a viscosity suitable..
Viscosity 17000 - 19000 cP
17000 - 19000 cP
Huntsman MY 9663 Multifunctional Resin
Weight per Epoxide (EEW, g/eq) 115 to 135. Color: BrownComments/Applications: Narrow viscosity MY 720. Used for high performance composites, adhesives, laminates and high energy radiation resistant..