Material Notes:
PVC Homopolymer Dispersion Resin F-34 is a medium molecular weight PVC homopolymer dispersion resin which has been developed primarily for use in chemically expanded compound. In expanded systems, the product exhibits a fine uniform cell structure in a variety of formulations and over a wide range of processing conditions.Note 1. 500 gm resin and 300 gm DOP, Hobart mixer mixed 5 min. @ No. 1 speed and 10 min. @ No. 2 speed, undeaerated.Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Volatiles 0.50 %
0.50 %
ASTM D3030
Viscosity 0.95 cP
0.95 cP
Inherent; ASTM D1243
13000 cP
13000 cP
Severs, 100 psig aged 2 hrs, See note 1; SPI-VD-T2
Relative Viscosity 2.25 cP
2.25 cP
QC-10-104
Brookfield Viscosity 10000 cP
10000 cP
20 rpm aged 2 hrs, See note 1; SPI-VD-T1
21000 cP
21000 cP
2 rpm aged 2 hrs, See note 1; SPI-VD-T1
Descriptive Properties Value Comments
Composition 0.025
Methanol Extract, ASTM D2222
Gelation Temperature 152°F
SPI-VD-T18
K-Value 67
Fikentscher's Constant