Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 5.0 - 10 g/10 min @Load 21.6 kg, Temperature 210 °C |
5.0 - 10 g/10 min @Load 47.6 lb, Temperature 410 °F |
cm<sup>3</sup>/10 min |
Huntsman IROGRAN® A 95 K 4640 TPU-For Seals Introduction: IROGRAN A95K 4640 is a caprolactone-based thermoplastic polyurethane. The material has been developed for injection molding applications requiring exceptional performance in terms of c.. |
|||
Melt Index of Compound | 5.0 - 10 g/10 min | 5.0 - 10 g/10 min | |
Sibur 21080-PM1 Polypropylene with Low Haze For production of three-layer PE/PP film, for production of sheets for cups and thin casting. It is allowed for contact with food products. |
|||
Melt Index of Compound | 5.0 - 10 g/10 min | 5.0 - 10 g/10 min | I Preparation |
Sibur ABS 2020 (30,31) Molding Grade ABS Plastic With high thermal and light resistance for automobile building, stable to atmospheric conditions in thermal and electric ageing, contacting with food products, as well as with compounding with PC. |
|||
Melt Index of Compound | 6.0 - 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.0 - 10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238, ISO 1133 |
EPICHEM Epilen PP 20GF NAT Polypropylene, 20% Glass Fiber Characteristics: 20% glass fibre filled |
|||
Melt Index of Compound | 6.0 - 10 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.0 - 10 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Arkema Group OREVAC® 18732 Grafted Maleic Anhydride Polypropylene OREVAC 18732 and 18732P are maleic anhydride grafted polypropylene used in the manufacturing of multiplayer structures. These products are available in pellets or in powder. OREVAC 18732 and 18732P .. |
|||
Melt Index of Compound | 6.0 - 10 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.0 - 10 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Arkema Group OREVAC® 18732P Grafted Maleic Anhydride Polypropylene OREVAC 18732 and 18732P are maleic anhydride grafted polypropylene used in the manufacturing of multiplayer structures. These products are available in pellets or in powder. OREVAC 18732 and 18732P .. |
|||
Melt Index of Compound | 8.0 - 10 g/10 min | 8.0 - 10 g/10 min | ASTM D1238 |
Cheng Yu Plastic IPS600UV Flame Retardant HIPS |
|||
Melt Index of Compound | 8.0 - 10 g/10 min | 8.0 - 10 g/10 min | ASTM D1238 |
Cheng Yu Plastic IPS600 Flame Retardant HIPS |
|||
Melt Index of Compound | 8.0 - 10 g/10 min | 8.0 - 10 g/10 min | ASTM D1238 |
Cheng Yu Plastic IPS601 Flame Retardant HIPS |
|||
Melt Index of Compound | 8.0 - 10 g/10 min | 8.0 - 10 g/10 min | ASTM D1238 |
Cheng Yu Plastic IPS620BK Electric Conducting HIPS, Injection |
|||
Melt Index of Compound | 8.0 - 10 g/10 min | 8.0 - 10 g/10 min | ASTM D1238 |
Cheng Yu Plastic IPS666N Electric Resisting HIPS |