Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 150 - 200 g/10 min @Load 2.16 kg, Temperature 190 °C |
150 - 200 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group LOTRYL® 28 BA 175 Copolymer Ethylene - Butyl Acrylate LOTRYL® 28 BA 175 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. Co-monomer content is 28% in weight. LOTRYL® 28 BA 175 is particularly.. |
|||
Melt Index of Compound | 150 - 200 g/10 min @Load 2.16 kg, Temperature 190 °C |
150 - 200 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group LOTRYL® 37 EH 175 Copolymer Ethylene - 2-Ethylhexyl Acrylate LOTRYL® 37EH175 is a random copolymer of Ethylene and 2-Ethylhexyl Acrylate, prepared by the high pressure polymerization process. LOTRYL® 37EH175 is particularly recommended for the formulation o.. |