Arkema Group LOTRYL® 37 EH 175 Copolymer Ethylene - 2-Ethylhexyl Acrylate

Category Polymer , Thermoplastic , Ethylene Acrylic Acid
Manufacturer Arkema
Trade Name LOTRYL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group LOTRYL® 37 EH 175 Copolymer Ethylene - 2-Ethylhexyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LOTRYL® 37EH175 is a random copolymer of Ethylene and 2-Ethylhexyl Acrylate, prepared by the high pressure polymerization process. LOTRYL® 37EH175 is particularly recommended for the formulation of hot melt adhesives.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.910 g/cc

@Temperature 23.0 °C
0.0329 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Index of Compound 150 - 200 g/10 min

@Load 2.16 kg,
Temperature 190 °C
150 - 200 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
ASTM D2240
Tensile Strength at Break 2.00 MPa
290 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Flexural Modulus 0.00500 GPa
0.725 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 73.0 °C
163 °F
DSC
Vicat Softening Point <= 40.0 °C

@Load 1.02 kg
<= 104 °F

@Load 2.25 lb
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F
Descriptive Properties Value Comments
2-Ethylhexyl Acrylate Content (%) 35-39
IRTF (internal)