Polymer Property : Melt Index of Compound = 2.4 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 1.8 - 2.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.8 - 2.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Petroquimica Triunfo Tritheva® PN 2021 EVA Copolymer
The Tritheva® PN 2021 resin is an Ethylene-Vinyl Acetate copolymer (EVA) mainly used for the production of crosslinked/expanded plates and other parts. This is an easy processing product with high ..
Melt Index of Compound 1.5 - 2.4 g/10 min
1.5 - 2.4 g/10 min
Sibur 21020-PM1 Polypropylene with Low Haze
For production of three-layer PE/PP film, for production of sheets for cups and thin casting. It is allowed for contact with food products.