Material Notes:
The Tritheva® PN 2021 resin is an Ethylene-Vinyl Acetate copolymer (EVA) mainly used for the production of crosslinked/expanded plates and other parts. This is an easy processing product with high compatibility with mineral fillers, other thermoplastic and elastomeric resins. Other important characteristics are elasticity, flexibility, excellent stress cracking resistance (ESCR), chemical resistance, and low temperature strength. The homogeneous morphology gives an outstanding crosslinkability for this resin, allowing for cost reduction by lower use of crosslinking agents and/or lower crosslinking time. The compounds obtained from the resin Tritheva® PN 2021 have the following properties: lightness, resistance to deformation, low shrink, high capacity of cementing and retention of colors.Applications: Shoe components such as soles, insoles, etc. Other expanded and/or crosslinked parts for several applications. Tubing and profiles. Polymeric blends and asphalt compounds.Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C.Information provided by Dax Resinas
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D1505
Vinyl Acetate Content 17.7 - 20.3 %
17.7 - 20.3 %
Melt Index of Compound 1.8 - 2.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.8 - 2.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
ASTM D2240
Tensile Strength at Break 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 750 %
750 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 86.0 °C
187 °F
ASTM D3418
Vicat Softening Point 61.0 °C
142 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 100 - 120 °C
212 - 248 °F
Mixture Zone