Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 0.20 - 0.50 g/10 min | 0.20 - 0.50 g/10 min | |
Sibur 23003-30T 1st Grade Polypropylene Copolymer For production of pipes for hot and cold water supply, sewerage, containers for shampoo, oil, milk, and packing products of low muddiness. |
|||
Melt Index of Compound | 0.20 - 0.50 g/10 min | 0.20 - 0.50 g/10 min | |
Sibur 23003-30T Superior Quality Polypropylene Copolymer For production of pipes for hot and cold water supply, sewerage, containers for shampoo, oil, milk, and packing products of low muddiness. |
|||
Melt Index of Compound | 0.20 - 0.90 g/10 min | 0.20 - 0.90 g/10 min | |
Sibur 23007-30T 1st Grade Polypropylene Copolymer For production of pipes for hot and cold water supply, sewerage, containers for shampoo, oil, milk, and packing products of low muddiness. |
|||
Melt Index of Compound | 0.20 - 0.90 g/10 min | 0.20 - 0.90 g/10 min | |
Sibur 23007-30T Superior Quality Polypropylene Copolymer For production of pipes for hot and cold water supply, sewerage, containers for shampoo, oil, milk, and packing products of low muddiness. |
|||
Melt Index of Compound | 0.20 - 1.0 g/10 min | 0.20 - 1.0 g/10 min | |
Sibur MPP 23007-E10 Frost Resistant Polypropylene For production of parts for automobiles (bumpers), accumulators, articles of technical purpose, including those electrical and exploited under low temperatures |
|||
Melt Index of Compound | 0.20 g/10 min | 0.20 g/10 min | Condition 190/2.16, Base; ASTM D1238 |
Chevron Phillips Marlex® M358Y3 LLDPE Pipe and Corrugated Extrusion Resin Characteristics: High visibility as gas pipingGood outdoor storage length when blended with natural MDPE containing UV stabilizerGood long-term hoop strengthApplications: PipesNot recommended for co.. |
|||
Melt Index of Compound | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow DGDA-2475 NT High Density Polyethylene Resin DOW DGDA-2475 NT is produced using UNIPOL™ process technology. It is intended for use in corrugated pipe applications. It has been specifically designed for extrusion of corrugated pipes with the.. |