Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 0.20 - 0.90 g/10 min | 0.20 - 0.90 g/10 min | |
Sibur 23007-30T 1st Grade Polypropylene Copolymer For production of pipes for hot and cold water supply, sewerage, containers for shampoo, oil, milk, and packing products of low muddiness. |
|||
Melt Index of Compound | 0.20 - 0.90 g/10 min | 0.20 - 0.90 g/10 min | |
Sibur 23007-30T Superior Quality Polypropylene Copolymer For production of pipes for hot and cold water supply, sewerage, containers for shampoo, oil, milk, and packing products of low muddiness. |