Physical Properties Metric English Comments
Melt Index of Compound 0.20 - 1.0 g/10 min
0.20 - 1.0 g/10 min
Sibur MPP 23007-E10 Frost Resistant Polypropylene
For production of parts for automobiles (bumpers), accumulators, articles of technical purpose, including those electrical and exploited under low temperatures